Hey Folks,
Next question. Wanted to try something a bit easier to sand than the pine flour I used on the pirogue last year as I have 10 seams to fillet this time rather than two :shock:
Picked up some phenolic microballons from Raka planning to use them on the fillets but now I'm reading that they shouldn't be used for structural fillets in more than a 25% concentration as they are not as strong as the wod flour or other fillers.
Opinions?
Thanks
Brad
Next question. Wanted to try something a bit easier to sand than the pine flour I used on the pirogue last year as I have 10 seams to fillet this time rather than two :shock:
Picked up some phenolic microballons from Raka planning to use them on the fillets but now I'm reading that they shouldn't be used for structural fillets in more than a 25% concentration as they are not as strong as the wod flour or other fillers.
Opinions?
Thanks
Brad